Properties | Tensile Strength | Yield Strength | Typical Yield | Typical Tensile | Yield strength & Yield point | Stainless Steel Tensile Strength | Bend Testing | Compression Testing | Difference Between Yield and Tensile | AISI Steel Yield Tensile | Strength Properties of Metals | Strength of Materials | Stress | Aluminum Mechanical Properties | Tensile Proof Stress Of Metric Bolts and Screws | Tensile Strength of Metric Nuts | Stainless Tensile Of Metric Bolts Screws | Physical Properties Stainless Steel Carbon Steel | Thermoplastics Physical Properties | British Standard Strength of Steel | Shear and Tensile | Elastic Properties Young Modulus | Stength European Standard | Ductility | Young’s Modulus | Non-Ferrous Modulus of Elasticity | Steel Bolts Strength | Iron Steel Modulus of Elasticity | Thermal Properties | Properties of Thermal | Thread Shear Calculator | Metals Properties | Stainless Steel Physical Properties | Definition Mechanical Properties
304 Stainless Steel Density:
0.285 lb/in³ (7.93kg/dm³)
Modulus of Elasticity in Tension:
29 x 106 psi (200 GPa)
Linear Coefficient of Thermal Expansion:
Temperature Range | Temperature Range | Coefficients | Coefficients |
°F | °C | in/in/°F | cm/cm/°C |
68 – 212 | 20 – 100 | 9.2 x 10-6 | 16.6 x 10-6 |
18 – 1600 | 20 – 870 | 11.0 x 10-6 | 19.8 x 10-6 |
Temperature Range | Temperature Range | Coefficients | Coefficients |
°F | °C | in/in/°F | cm/cm/°C |
68 – 212 | 20 – 100 | 9.2 x 10-6 | 16.6 x 10-6 |
18 – 1600 | 20 – 870 | 11.0 x 10-6 | 19.8 x 10-6 |
The overall heat transfer coefficient of metals is determined by factors in addition to the thermal conductivity of the metal. The ability of the 18-8 stainless steel grades to maintain clean surfaces often allows better heat transfer than other metals having higher thermal conductivity.
Specific Heat:
°F | °C | Btu/lb/°F | J/kg/K |
32 – 212 | 0 – 100 | 0.12 | 500 |
Magnetic Permeability:
The 18-8 alloys are generally non-magnetic in the annealed condition with magnetic permeability values typically less than 1.02 at 200H. Permeability values will vary with composition and will increase with cold work.
Percent Cold Work | Magnetic Permeability | |
304 | 304L | |
0 | 1.005 | 1.015 |
10 | 1.009 | 1.064 |
30 | 1.163 | 3.235 |
50 | 2.291 | 8.480 |
Physical Properties of Stainless SteelGeneral Properties