The American Society for Testing Materials (ASTM) numbering system for grey cast iron is established such that the numbers corespond to the minimum tensile strength in kpsi. Thus an ASTM no. 20 cast iron has a minimum tensile strength of 20 kpsi. Note particularly that the tabulations are typical values. Multiply strength in kpsi be 6.89 to get strength in MPa.