410 Physical Properties
The values reported below are typical for Alloy 410 in the annealed condition.
Modulus of Elasticity:
29 x 106 psi (200 GPa)
Specific Gravity:
7.65
Density:
0.276 Lbs/in3
Specific Heat:
.11 Btu/lb. ∑ °F
Thermal Conductivity at 212°F (100°C):
14.4 Btu/(hr ∑ ft ∑ °F)
24.9 W/m ∑ K
Electrical Resistivity:
56 Microhm-cm 68°F (20°C)
Coefficient of Thermal Expansion:
68 - 392°F, 5.9 x 10-6 in/in°F
20 - 200°C, 10.5 x 10-6 cm/cm/°C
68 - 1112°F, 6.5 x 10-6 in/in/°F
20 - 600°C, 11.6 x 10-6 cm/cm/°C
Melting Range:
2700 - 2790°F
1482 - 1532°C