For maximum
corrosion resistance to chemical environments, it is essential that the 410S surface be free of all heat tint or oxide formed during annealing or hot working. All surfaces must be ground or polished to remove any traces of oxide and surface decarburization. The parts should then be immersed in a warm solution of 10-20% nitric acid followed by a water rinse to remove any residual iron.