All common welding methods used for stainless steel will be successful with 430. Filler metal should be AWS E/ER308 or 312
If welding is necessary pre-heat at 150-200°C. Embrittlement in the weld metal and heat affected zone can be relieved by a post-weld anneal at 790-815°C, but grain refinement will not occur. Use Grade 430, 308L, 309 or 310 filler rod, depending upon application. AS 1554.6 pre-qualifies welding of Grade 430 with Grade 309 filler rods and electrodes.